Master Bond tested epoxies from our line of chemically resistant compounds for their ability to resist exposure to DMSO (dimethyl sulfoxide). Ten of our top performing compounds were cured and then immersed in DMSO (some for over a 2.5 year span) while weekly measurements were recorded to assess the percentage of weight change from start to finish. See the results of our best performing DMSO resistant adhesives.
Top Adhesive Systems with DMSO Resistance
EP46HT-2AO Black
Two part, NASA low outgassing approved epoxy system