                              | The Rigors of 85°C + 85% Humidity Testing for Adhesives | 
                             
                            
                            
                               | 
                             
                            
                            
                              | Master Bond has selected a group of adhesive compounds for testing at 85°C and 85% relative humidity which can help determine the expected operating life for the devices they are utilized in. The test requires hardness measurements of the cured castings before and after exposure to determine which products performed best. Click below to learn more about the testing process and to see a full list of compounds that passed the rigorous requirements. | 
                             
                            
                            
                               | 
                             
                            
                            
                              | 
                                
                               | 
                             
                            
                           
                         | 
                       
                      
                         | 
                       
                     
                   | 
                 
               
             | 
           
          
             | 
           
         
       | 
     
   
  
  
  
    
      
        
          
            
              
                
                  
                    
                      
                         | 
                       
                      
                      
                        | 85°C/85%RH Tested Adhesive Systems | 
                       
                      
                      
                         | 
                       
                      
                      
                        | 
                          
                         | 
                       
                      
                     
                   | 
                 
               
             | 
           
         
       | 
     
   
  
  
   
  
    
      
        
          
            
              
                
                  
                    
                      
                         | 
                       
                      
                        
                          
                          
                          
                          
                          
                          
                            
                              
                                
                                  
                                    
                                    
                                      | MasterSil 151 | 
                                     
                                    
                                    
                                       | 
                                     
                                    
                                    
                                      | Flexible, low viscosity addition curing silicone compound | 
                                     
                                    
                                    
                                       | 
                                     
                                    
                                    
                                      | 
                                        
                                       | 
                                     
                                    
                                    
                                       | 
                                     
                                   
                                 | 
                               
                             
                           
                          
                          
                         
                         | 
                       
                     
                   | 
                 
               
             | 
           
         
       | 
     
   
  
  
 
 
 
     
  
    
      
        
          
            
              
                
                  
                    
                      
                         | 
                       
                      
                        
                          
                          
                          
                          
                          
                          
                            
                              
                                
                                  
                                    
                                    
                                      | EP79 | 
                                     
                                    
                                    
                                       | 
                                     
                                    
                                    
                                      | Electrically & thermally conductive silver coated nickel epoxy | 
                                     
                                    
                                    
                                       | 
                                     
                                    
                                    
                                      | 
                                        
                                       | 
                                     
                                    
                                    
                                       | 
                                     
                                   
                                 | 
                               
                             
                           
                          
                          
                         
                         | 
                       
                     
                   | 
                 
               
             | 
           
         
       | 
     
   
  
     
  
    
      
        
          
            
              
                
                  
                    
                      
                         | 
                       
                      
                        
                          
                          
                          
                          
                          
                          
                            
                              
                                
                                  
                                    
                                    
                                      | EP42HT-2AO-1 Black | 
                                     
                                    
                                    
                                       | 
                                     
                                    
                                    
                                      | Cryogenically serviceable epoxy with superior thermal stability | 
                                     
                                    
                                    
                                       | 
                                     
                                    
                                    
                                      | 
                                        
                                       | 
                                     
                                    
                                    
                                       | 
                                     
                                   
                                 | 
                               
                             
                           
                          
                          
                         
                         | 
                       
                     
                   | 
                 
               
             | 
           
         
       | 
     
   
  
 
  
    
      
        
          
            
              
                
                  
                    
                      
                         | 
                       
                      
                        
                          
                          
                          
                          
                          
                          
                            
                              
                                
                                  
                                    
                                    
                                      | Supreme 10AOHT-LO | 
                                     
                                    
                                    
                                       | 
                                     
                                    
                                    
                                      | NASA low outgassing approved high strength epoxy | 
                                     
                                    
                                    
                                       | 
                                     
                                    
                                    
                                      | 
                                        
                                       | 
                                     
                                    
                                    
                                       | 
                                     
                                   
                                 | 
                               
                             
                           
                          
                          
                         
                         | 
                       
                     
                   | 
                 
               
             | 
           
         
       | 
     
   
  
 
  
    
      
        
          
            
              
                
                  
                    
                      
                         | 
                       
                      
                        
                          
                          
                          
                          
                          
                          
                            
                              
                                
                                  
                                    
                                    
                                      | UV22 | 
                                     
                                    
                                    
                                       | 
                                     
                                    
                                    
                                      | Abrasion resistant, UV curable nanosilica filled adhesive | 
                                     
                                    
                                    
                                       | 
                                     
                                    
                                    
                                      | 
                                        
                                       | 
                                     
                                    
                                    
                                       | 
                                     
                                   
                                 | 
                               
                             
                           
                          
                          
                         
                         | 
                       
                     
                   | 
                 
               
             | 
           
         
       | 
     
   
  
 
  
    
      
        
          
            
              
                
                  
                    
                      
                         | 
                       
                      
                        
                          
                          
                          
                          
                          
                          
                            
                              
                                
                                  
                                    
                                    
                                      | EP21TDC-2LO | 
                                     
                                    
                                    
                                       | 
                                     
                                    
                                    
                                      | Flexible, low outgassing epoxy with high thermal conductivity | 
                                     
                                    
                                    
                                       | 
                                     
                                    
                                    
                                      | 
                                        
                                       | 
                                     
                                    
                                    
                                       | 
                                     
                                   
                                 | 
                               
                             
                           
                          
                          
                         
                         | 
                       
                     
  |  
                                       | 
                                     
                  
                
               
             | 
           
         
       | 
     
   
  
  
  
  
  
   
  
    
      | 
        
       | 
     
    
      
        
          
             | 
           
          
            
              
              
              
 
              
              
                
                  | 