
Master Bond's high performance one and two component industrial sealants are easy to apply and are available for use in convenient applicators. They provide cost effective solutions for high tech applications. Our sealing products consist of epoxies, silicones, polysulfides and polyurethanes. They are 100% reactive and contain no solvents or diluents.
| Product Chemistry | Typical Properties |
|---|---|
| Epoxies |
|
| Silicones |
|
| Urethane modified epoxies |
|
| Polysulfide modified epoxies |
|
| UV/LED curables |
|
Low/medium/high viscosity liquid elastomeric systems including pastes provide safe, reliable protection against dust, dirt, fluids, gases, contaminants. These high elongation compounds exhibit good weathering characteristics, aging properties and offer resistance to cracking, blistering, and embrittlement under harsh conditions. Most noteworthy is their ability to withstand vibration, shock, impact, heating/cooling cycles, humidity. Select durable, flexible compounds have proven effective in sealing dissimilar substrates and joints subjected to high/moderate cyclic movement even at low temperatures. Additionally systems have been developed for damp conditions, chemical attack, abrasion and wear. Multipurpose sealants offer fast fixture speeds, low shrinkage, gap filling, good electrical insulation for interior/exterior use. They have proven successful in guarding key components against high pressure.
Common Applications for Master Bond's Industrial Sealants
Our formulations are used in a wide range of industries including aerospace, electronic, appliance, oil/chemical processing, medical, optical, etc. They are involved in various sealing applications including:
- Hatches
- Semiconductor electronics
- Thermostats
- Optical devices
- MEMS
- Switches
- Pipe joints carrying corrosive chemicals
- Modules and housings
- Pumps
- Industrial ovens
Our Most Popular Sealant Formulations
|
FLM36 B-staged film adhesive/sealant. Outstanding thermal cycling capabilities and structural properties. Offers superior toughness and flexibility. Excellent strength retention at elevated temperatures. Thermally conductive/electrically insulative. Provides uniform bond line thickness. Serviceable from -100°F to +500°F. Preforms are available. |
|
EP30ND Light paste. Spreads evenly and smoothly. Superior chemical resistance properties. Cures at room temperatures. Machinable. Service temperature range -60°F to +250°F. High bond strength |
|
EP30P Two part, room temperature curing epoxy system with excellent optical transparency. Low viscosity. Bonds extremely well to more sensitive plastics such as polycarbonates and acrylics. Superior electrical insulation properties. Good chemical resistance to oils, fuels, water, hydraulic fluids. Serviceable from -60°F to +250°F. |
|
UV18S UV curable system with superior resistance to chemicals, particularly solvents. High bond strength. Excellent light transmission properties. Electrical insulator. Low shrinkage upon cure. Exceptionally fast curing. Serviceable from -60°F to 250°F. |
|
MasterSil 153 Two part silicone paste for bonding and sealing applications. Outstanding flexibility. Low exotherm and long pot life system. Self priming feature. Contains no solvents or diluents. Superior electrical insulation properties. Can cure in wide sections vertically and horizontally. Serviceable from -65°F to +400°F |
|
EP30DPSP Epoxy-urethane blend. Superior toughness and abrasion resistance. Biocompatible. Cryogenically serviceable. Low viscosity. Low moisture absorption and hydrolytic stability. USP Class VI approved. Serviceable from 4k to +250°F. Outstanding electrical insulation properties. Withstands thermal cycling. High impact strength. |
|
Supreme 34CA Serviceable from -80°F to +500°F. Good flow properties. Two component epoxy system. Impressive resistance to aggressive chemicals. Oven curing. Structural adhesive. Superior electrical insulator. Used for filament winding, bonding composites, pultruded structures. |






