Some of the vital properties for the assembly of respiratory devices such as ventilators in the medical industry include but are not limited to good strength, fast processing speeds, and in many cases a high degree of flexibility. Master Bond’s line of USP Class VI and ISO 10993-5 certified adhesives, sealants, and coatings not only meet stringent biocompatibility requirements, but also pass rigorous cytotoxicity tests. These products can be used to bond a variety of substrates ranging from polycarbonates, acrylics, polyesters, to other plastics, metals, ceramics, and various electronic components. They are environmentally friendly, and many of them contain no solvents or diluents. These products are resistant to a wide range of sterilants, chemicals, and temperatures.
Some examples of products include:
| Products | Certifications | Key Features | 
| UV15X-6Med-2 | USP Class VI & ISO10993-5 rated, one component UV curable system | Good degree of flexibility Fast cure speeds | 
| EP21LV3/5Med | USP Class VI rated, two component room temperature curable epoxy | High elongation Good bond strength | 
| X21Med | ISO10993-5 rated one component primer/adhesive | Primer/adhesive for Polyolefins Good degree of toughness | 
| UV22DC80-1Med | USP Class VI & ISO rated 1 component UV + heat or dual curing epoxy | Nano-silica filled Good dimensional stability | 
| MasterSil 912Med | USP Class VI & ISO rated 1 component silicone | High degree of flexibility Paste consistency | 
These products are widely used for bonding, sealing, and encapsulation applications for filters, valves, tubes, cartridges, regulators, sensors, gaskets, and face shields, which are eventually used as components needed for respiratory devices.
Medical Grade Adhesives for Respiratory Devices Assembly
|   | UV15X-6Med-2 UV curing system with high flexibility that is biocompatible per USP Class VI testing. Medium viscosity. Superior abrasion resistance. Non-yellowing. Reliable thermal and electrical insulator. Serviceable from -80°F to +250°F. | 
|   | EP21LV3/5Med Low viscosity epoxy adhesive, sealant, coating and casting compound. USP Class VI approved. Resists vibration, impact, shock., thermal cycling. Ideally suited to bond dissimilar substrates. Serviceable from -80°F to +250°F. Withstand exposure to EtO, radiation and chemical sterilants. Excellent toughness. | 
|   | X21Med Specially formulated one component system for bonding and priming polyolefinic surfaces. Can be used as a primer to promote adhesion of polyolefinic substrates to other surfaces such as metals, ceramics. Viscosit <250 cps. Room temperature curing. Serviceable from -60°F to +200°F. Passes ISO 10993-5 for medical devices. | 
|   | UV22DC80-1Med Dual cure system with UV and heat curing mechanisms. Cures at 80°C in shadowed out areas. Nano filled, high dimensional stability and abrasion resistance. Bonds well to metals, glass, ceramics and most plastics. Serviceable from -60°F to +350°F. | 
|   | MasterSil 912Med Single component silicone with a paste viscosity for bonding, sealing and coating medical devices. Non-corrosive, neutral cure compound complies with USP Class VI and ISO 10993-5 specifications. Resists many kinds of sterilization including gamma and other types of radiation, EtO and some types of liquid sterilants. | 
 
			      