Properties of Polysulfide Modified Epoxy Adhesive Systems
- Exceptional chemical resistance
 - High dielectric strength
 - High physical strength
 - High and low temperature serviceability
 - Resistance to vibration, impact, shock and thermal cycling
 - Metal free
 - Long-term resistance to gasoline, natural gas, gaseous fuels, kerosene, alcohol, crude oils and its derivatives
 - Easy application
 - Excellent adhesion to similar and dissimilar substrates
 
Applications of Polysulfide Modified Epoxy Adhesives
Master Bond polysulfide modified epoxies are versatile synthetic elastomers that are used in the aerospace, electronic, electrical, computer, metalworking, appliance, automotive, oil & gas, electric vehicle and chemical industries. They can be used in a wide range of applications, such as:
- Aircraft fuel tank sealants
 - Industrial tank liners
 - Electrical potting
 - Corrosion protection of offshore structures
 - Vibration resistance of electro-optical devices
 
Most Popular Polysulfide System Products
                        | 
                  
            EP21TPND-NV Two part, room temperature curing polysulfide paste. Excellent for bonding and sealing in fuel and oil environments. Forgiving one to one mix ratio by weight or volume. Service operating temperature range from -80°F to +250°F. Resists rigorous thermal cycling. Superior electrical insulation properties.  | 
              
                        | 
                  
            EP21TPFL-1AO Two part, room temperature curing, very flexible polysulfide system with excellent thermal conductivity. Low viscosity and good flowability for potting and encapsulating applications. Superior electrical insulation characteristics. Withstands thermal cycling. Reliable resistance to fuels and oils. Long open time. Serviceable from -60°F to +250°F.  | 
              
                        | 
                  
            EP21TPHT Two component polysulfide/epoxy adhesive/sealant. Cures at room or elevated temperature. Exceptional toughness and chemical resistance properties. Withstands exposure to fuels, oils, hydrocarbons and hydraulic fluids. One to one mix ratio by weight or vollume. Excellent electrical insulation properties. Serviceable from -80°F to +350°F.  | 
              
                        | 
                  
            EP21TP-2NV Two component polysulfide/epoxy adhesive/sealant. Cures at room or elevated temperature. Exceptional toughness and chemical resistance properties. Withstands exposure to fuels, oils, hydrocarbons and hydraulic fluids. Forgiving one to one mix ratio. Excellent electrical insulation properties. Serviceable from -80°F to +250°F.  | 
              
			      