One Component, Heat Curing, High Purity Nickel Conductive Epoxy Adhesive/Sealant Featuring Both High Shear and High Peel Strength for Performance up to 400°F
One Component, Silver Conductive Epoxy Adhesive Featuring High Shear and High Peel Strengths. Uniquely Special System Cures between 175°F and 185°F with Physical Strength Properties and Excellent Conductivity.
One Component, Heat Curing, Silver Filled, Electrically Conductive Epoxy Adhesive/Sealant Featuring High Shear Strength and Good Temperature Resistance Along With a Rapid Cure Speed.
One Component, Heat Curing, Silver Filled, Electrically Conductive Epoxy Adhesive/Sealant Featuring High Shear Strength and Good Temperature Resistance Along With a Rapid Cure Speed.
Two Component Nickel Conductive Epoxy Adhesive for High Performance Bonding Featuring High Peel Strength, Superior Toughness and Low Volume Resistivity
One Component, Heat Curing, Silver Filled, Electrically Conductive Epoxy Adhesive/Sealant Featuring High Shear Strength and Good Temperature Resistance Along With a Rapid Cure Speed.