Supreme 10HTF-1 Product Information | MasterBond.com

One component, fast curing, toughened epoxy adhesive/sealant

Supreme 10HTF-1 One Part Epoxy Compound

Key Features

  • Convenient processing and fast curing
  • Exceptionally high bonding strength
  • Serviceable from 4K to +400°F
  • Can withstand rigorous thermal cycling