27 products match
|
MasterSil 410 Non-sag acetoxy type silicone. Provides protection against vibration and shock. Superb weatherability. Elongation 600%. Serviceable from -75°F to 400°F. |
|
MasterSil 415 Optically clear, room temperature curing, no mix acetoxy type system. Good bond strength and outstanding elasticity. Serviceable from -185°F to 400°F. |
|
MasterSil 702 Non-corrosive, high performance elastomeric adhesive/sealant. Heat resistant up to 450°F. Superior physical strength properties. Electrically insulative. |
|
MasterSil 705 Translucent flowable paste for bonding, sealing, coating, formed-in-place gaskets. Cures upon exposure to atmospheric moisture. Serviceable from -75°F to 400°F. Available in tubes, cartridges. |
|
MasterSil 705C Single component, electrically conductive, non-corrosive silicone compound. Carbon filled. Tack free time 3-7 minutes at ambient temperatures. Paste viscosity. Serviceable up to 400°F. |
|
MasterSil 705S Silver filled, one-part, no-mix, non-corrosive silicone system. Shore A hardness 70. Cures at room temperatures when exposed to atmospheric moisture. Extremely low volume resistivity. Most effective when applied in thin sections. |
|
MasterSil 705TC Thermally conductive and electrically isolating. Easy to use silicone for high performance bonding, sealing and coating. Non-corrosive and room temperature curable. Ideally suited for applications requiring flexibility and high temperature resistance. |
|
MasterSil 707FR-NV One component non-corrosive paste produces fast cures at room temperature. Passes UL 94V-1 and 94V-0 testing for flame retardancy. Outstanding adhesion to metals, ceramics, glass and many plastics. Exceptionally soft. |
|
MasterSil 708FR Flowable, no mix, one component RTV silicone compound. Shore A Hardness 30-40. Fast setting at room temperature. Meets requirements of UL 94V-1 and 94V-0 for flame retardancy. Elongation of 200-300%. Gray color. |
|
MasterSil 709 One component, fast curing, moderate viscosity silicone elastomer compound for bonding, sealing, coating and formed in place gaskets. Non-corrosive and flowable. Bonds well to a variety of surfaces and substrates. Servicable from -75°F to +400°F. Meets MIL-A-46146 Type 2. |