188 products match
|
Supreme 10AOHT One part, oven cured epoxy system with excellent thermal conductivity and superb resistance to thermal cycling. Primarily used for bonding of heat sinks and sensors where heat transfer is desirable. Serviceable from 4k to +400°F. Convenient processing. |
|
Supreme 10AOHT-LO Thermally conductive and electrically insulative, one part epoxy adhesive. Superior toughness and dimensional stability. Bonds are resistant to thermal cycling and many chemicals. Serviceable from 4K to +400°F. NASA low outgassing approved. Withstands 1,000 hours 85°C/85% RH. Impressive physical strength properties. |
|
Supreme 10HTN-NV High peel and shear strength single component nickel filled epoxy adhesive. Thixotropic system. Cost effective electrical conductivity. Resists from 4k to +400°F. |
|
Supreme 10HTS Silver filled system with excellent electrical conductivity and high physical strength properties. One part, heat cured (250-300°F) epoxy. Wide range of serviceability from cryogenic temperatures up to +400°F. Meets NASA low outgassing specifications. Can be applied without sagging or dripping, even on vertical surfaces. Volume resistivit <0.006 ohm-cm. Thermally conductive. Shore D hardnes >75. |
|
Supreme 11AN Epoxy adhesive features outstanding thermal conductivity. Superb electrical insulation properties. Tough bonds. High shear and peel strength. Cures at ambient temperatures. Low CTE. Paste viscosity. Serviceable from -100°F to +250°F. |
|
Supreme 11ANHT High temperature resistant epoxy for bonding and sealing. Toughened formulation. Superior shear/peel strength. Excellent heat transfer properties. Superb dielectric characteristics, Serviceable from -112°F to +400°F. |
|
Supreme 11ANHT-2 High temperature resistant epoxy for bonding, coating and sealing. Toughened formulation. Withstands thermal cycling. Excellent heat transfer properties. Small particle size allows for thin bond lines and low thermal resistance. Serviceable from -112°F to +400°F. |
|
Supreme 11AO Thermally conductive/electrically isolating epoxy adhesive/sealant. Ambient temperature curing. Convenient one to one mix ratio by weight or volume. Thick paste. High peel and shear strength. Toughened system. Well suited for bonding dissimilar substrates. Service temperature range -100°F to +250°F. |
|
Supreme 11AOHT Thermally conductive, electrically insulative epoxy adhesive. Meets MIL-STD-883J Section 3.5.2 for thermal stability. High peel and shear strength properties. Non-drip system. Resists -112°F to +400°F. Toughened system. Can withstand rigorous thermal cycling. Convenient one to one mix ratio by weight or volume. Cures at room temperature. |
|
Supreme 11AOHT-LO Passes NASA low outgassing tests. Thixotropic paste viscosity. Convenient one to one mix ratio by weight or volume. High thermal conductivity. Excellent electrical insulation properties. Dimensionally stable. Withstands 1,000 hours 85°C/85% RH. Toughened system. Ability to resist rigorous thermal cycling. Service temperature range -112°F to +400°F. |