442 products match
|
EP3HTMed Rapid curing, one part epoxy. Meets USP Class VI biocompatibility standards. Thixotropic paste viscosity. High shear strength. Superb resistance to autoclaving, chemical sterilants, radition, EtO. Serviceable from -60°F to +400°F. |
|
EP3HTND-2 Black Rapid curing, one part epoxy. Meets USP Class VI biocompatibility standards. Non-drip, paste viscosity. High shear strength. Superb resistance to autoclaving, chemical sterilants, radition, EtO. Serviceable from -60°F to +400°F. |
|
|
EP3HTND-2Med Black Rapid curing, one part epoxy. Meets USP Class VI biocompatibility standards. Non-drip, paste viscosity. High shear strength. Superb resistance to autoclaving, chemical sterilants, radition, EtO. Serviceable from -60°F to +400°F. |
|
EP3LV One component heat curing epoxy adhesive. Outstanding dimensional stability. Does not contain any solvents or diluents. Superior tensile shear strength. Adhesive spreads evenly and smoothly. Easy to dispense. Thermal insulator. Serviceable from -100°F to +300°F. |
|
EP3SP5FL Single component snap cure adhesive. Unsurpassed curing speed of 1-2 minutes at 300°F. Moderate viscosity with good flow properties. Easy to dispense. Good tensile lap shear strength. Repairable. Serviceable from -60°F to +200°F. |
|
EP3SP5FL-ND2 Snap cure epoxy adhesive. Paste viscosity. Cures in 1-2 minutes at 300°F. Readily reworkable. Good bond strength and electrical insulation properties. Serviceable from -60°F to +200°F. |
|
EP40 Excellent adhesion to metals and engineering plastics such as polycarbonates, acrylics. Flexible. Low to moderate viscosity bonding, potting, sealing, encapsulation compound. High shear/peel strength. Resists mechanical shocks and vibration. Moderately low exotherm during cure. Serviceable from -80°F to +250°F. |
|
EP40Med Excellent adhesion to metals and engineering plastics such as polycarbonates, acrylics. Flexible. Low to moderate viscosity bonding, potting, sealing, encapsulation compound. High shear/peel strength. Resists mechanical shocks and vibration. Moderately low exotherm during cure. Serviceable from -80°F to +250°F. |
|
EP40ND Excellent adhesion to metals and engineering plastics such as polycarbonates, acrylics. Flexible. For bonding, potting, sealing compound. High shear/peel strength. Resists mechanical shocks and vibration. Moderately low exotherm during cure. Serviceable from -100°F to +250°F. Paste consistency. |
|
EP40NDMed Excellent adhesion to metals and engineering plastics such as polycarbonates, acrylics. Flexible. For bonding, potting, sealing compound. High shear/peel strength. Resists mechanical shocks and vibration. Moderately low exotherm during cure. Serviceable from -100°F to +250°F. Paste consistency. Meets ISO 10993-5 for cytotoxicity. |