630 products match
|
EP13 One component, heat curable epoxy adhesive. Serviceable from -60°F to +500°F. Paste viscosity. High tensile shear and compressive strength. Chemical resistant. Machinable. |
|
EP132 Two part high temperature resistant epoxy system. Capable of service up to 550°F. 100% reactive. Unmatched durability. Outstanding electrical and physical strength properties. Service operating temperature range from -60°F to +550°F. |
|
EP13LTE One component, heat curable epoxy adhesive. Serviceable from -60°F to +500°F. Paste viscosity. High tensile shear and compressive strength. Chemical resistant. Machinable. Low coefficient of thermal expansion. Meets NASA low outgassing standards. |
|
EP13SPND-2 Non-drip single component adhesive. Will not flow when cured. Serviceable up to +500°F. Electrically insulative. Withstands 1000 hours 85°C/85%RH. Excellent bond strength properties. |
|
EP15 No mix compound has exceptional tensile strength properties. Superior dimensional stability. Used for testing the adhesion and/or cohesive strength of flame sprayed coating per ASTM C633. Low shrinkage upon cure. Viscosity 40,000-65,000 cps. Serviceable from -60°F to +250°F. |
|
EP15ND-2 No mix compound has exceptional tensile strength properties. Superior dimensional stability. Used for testing the adhesion and/or cohesive strength of flame sprayed coating per ASTM C633. Low shrinkage upon cure. Viscosity 40,000-65,000 cps. Serviceable from -60°F to +250°F. |
|
EP17HT Serviceable up to 600°F. Exceptional Tg of 220-225°C. No mix formulation. Low exotherm upon curing. Exemplary chemical resistance. Can be used in encapsulations and castings beyond 1/2 inch thickness. |
|
EP17HT-100 High performance one part epoxy. Good flow properties. Thermally conductive, electrically insulative. Service temperature range -100°F to +500°F. Can be cast in thicknesses up to 1/2 inch. High dimensional stability. |
|
EP17HT-3 One part snap cure epoxy. Cures in 2-3 minutes at 250-300°F. Service operating temperature range -60°F to +400°F. Ideal for bonding dissimilar substrates and applications subject to thermal cycling. Outstanding electrical insulation properties. Withstands 1000 hours at 85°C/85%RH. |
|
EP17HT-LO One part, no mix epoxy meets NASA low outgassing specifications. Serviceable up to 600°F. Tg is 225°C. High shear, tensile and compressive strength properties. Cures in 90-120 minutes at 300F. Withstands 1000 hours 85°C/85% RH. |