EP51 "5" minute type system. Fast setting. Rapid curing at ambient temperature. Serviceable from 4K to +250°F. Adhesive/sealant. High strength bonds. Good chemical resistance. One to one mix ratio weight or volume. |
|
EP51AN Rapid room temperature curing thermally conductive/electrically insulative adhesive. Fast gelling. Low CTE. Serviceable from 4K to +250°F. High bond strength. Superior heat dissipative properties. Dimensionally stable. Chemical resistant. |
|
EP51AO Rapid curing epoxy adhesive/sealant. Excellent thermal conductivity/electrical insulative properties. Fast set up time. Convenient one to one mix ratio by weight or volume. Serviceable from 4K to +250°F. Resists water, oil, fuels and many solvents. Superior heat dissipation characteristics. |
|
EP51CC Easy to apply, paste like consistency two component epoxy adhesive. High bond strength. Can be packaged for use in field applications. Serviceable at cryogenic temperatures down to 4K. |
|
EP51FL Tough, flexible epoxy adhesive cures rapidly at ambient temperatures. High bond strength. Cryogenically serviceable. Easy to use, one to one mix ratio. |
|
EP51FL-1 Flexible epoxy adhesive has rapid set up time and cure speed. High peel strength and elongation. Withstands mechanical shock and vibration. Resists thermal cycling. Superb electrical insulation properties. Service operating temperature range from -100°F to +250°F. |
|
EP51FL-1ND-2 Flexible epoxy adhesive has rapid set up time and cure speed. High peel strength and elongation. Withstands mechanical shock and vibration. Resists thermal cycling. Superb electrical insulation properties. Service operating temperature range from -100°F to +250°F. |
|
EP51HT Service operating temperature range from 4K to +400°F. Fast room temperature curing epoxy adhesive/sealant. Gels in 5 minutes. Convenient one to one mixing ratio by weight. Bonds well to similar/dissimilar substrates. High tensile lap shear strength. |
|
EP51M Rapid curing at room temperature. Fixturing period 7-12 minutes. Convenient one to one mix ratio by weight or volume. High bond strength and long term durability. Withstands 1,000 hours 85°C/85% RH. Serviceable from 4k to +250°F. Available in various viscosities and colors. |
|
EP51ND High viscosity paste. Does not drip on vertical surfaces. Fast "5 minute" curing, two component epoxy adhesive. High bond strength. Serviceable from -100°F to +250°F. Superior durability. One to one mix ratio weight or volume. Excellent dielectric properties. |