439 products match
Supreme 30 Low viscosity, toughened, two component epoxy adhesives. High strength system. Superior durable. Adheres well to similar/dissimilar substrates. Serviceable from -60°F to +250°F. Exceptionally low shrinkage upon cure. Ambient temperature curing formulation. |
|
Supreme 33 Thermally stable, toughened, two component epoxy adhesive, sealant, coating. Serviceable from -80°F to +425°F. Good strength retention at elevated temperatures. Superior durability. Withstands thermal cycling. Chemical resistant. Ambient temperature curing. One to one mix ratio by volume. |
|
Supreme 33CLV Two component, room temperature curing structural epoxy system. Excellent bonding properties. Superior thermal cycling capabilities. Convenient one to one mix ratio by volume. Moderate viscosity. Toughened system. Outstanding resistance to water, fuels, various solvents acids and bases. Shore D hardness 75-80. |
|
Supreme 33ND Toughened, two component, non-drip epoxy adhesive, sealant, coating. Gap filling. Temperature range from -80°F to +425°F. Thermal shock and chemical resistant. Excellent durability and dimensional stability. Minimal shrinkage upon curing. Solid electrical insulator. Withstands 1,000 hours 85°C/85% RH. |
|
Supreme 34CA Serviceable from -80°F to +500°F. Good flow properties. Two component epoxy system. Impressive resistance to aggressive chemicals. Oven curing. Structural adhesive. Superior electrical insulator. Used for filament winding, bonding composites, pultruded structures. |
|
Supreme 3HT One part, oven curing epoxy system with very good adhesion to a wide range of plastics. Especially well suited for bonding dissimilar plastic materials. Resists -100°F to +350°F. Exceptional toughness. Successfully tested for 1,000 hours at 85°C/85% RH. |
|
Supreme 3HT-80 Fast cures at ambient 175°F (80°C). Recommended for bonding heat sensitive substrates. Outstanding thermal cycling capabilities. Single part no mix system. Serviceable from -100°F to +350°F. Tough and durable. Withstands 1,000 hours at 85°C/85% RH. |
|
Supreme 3HTLV One part, lower viscosity, oven curing epoxy system with very good adhesion to a wide range of plastics. Especially well suited for bonding dissimilar plastic materials. Resists -100°F to +350°F. Exceptional toughness. |
|
Supreme 42HT-2 High temperature resistant epoxy adhesive. Toughened. Excellent bond strength. Withstands exposure to many acids, bases, solvents, fuels and oils. Easy application. Service temperature range -80°F to +450°F. Good flow properties. Low exotherm. Long working life. Reliable electrical insulator. Resists thermal cycling. |
|
Supreme 42HT-2ND Non-drip epoxy paste has outstanding temperature and chemical resistance. Superior toughness and thermal cycling capability. Meets low outgassing specifications. Withstands 1,000 hours 85°C/85% RH. Superb electrical insulator. Service temperature range -80°F to +450°F. |