10 products match
|
EP21FRNS-2 Durable potting, encapsulation, casting compound meets UV 94V-0 flame retardant specifications. Convenient one to one mix ratio by weight. Features a non-halogen filler. Superb flow properties. Outstanding electrical insulation. Low smoke generation. Serviceable from -51°C to +90°C. |
|
EP36FR Flame retardant B-stage toughened epoxy. One part system. Ideal for potting and encapsulation. Capable of withstanding rigorous thermal shocks. Serviceable from -100°F to +500°F. Available in 30 gram cookies. |
|
EP90FR-H Two component high strength flame retardant epoxy system. Meets stringent horizontal burn test portion of the FAR standard 14 CFR 25.853(a). Non-halogenated System. Forgiving one to one mix ratio by weight. Good electrical insulation. Serviceable from -60°F to +250°F. Low shrinkage. |
|
EP90FR-HFL Toughened epoxy system complies with FAR standard 14CFR 25.853(a) for flame retardancy. Bonding, sealing, coating, potting compound. Passes horizontal burn test specification. Withstands mechanical shock and vibration. Thermal cycling resistant. Non-halogenated type system. Bonds well to dissimilar substrates. Serviceable from -60°F to +250°F. Impressive electircal insulator. |
|
EP90FR-V Two part epoxy passes vertical burn test portion of FAR standard 14 CFR 25.853(a) for flame retardancy. Passes Boeing standard BSS 7238, Revision C for low smoke and BSS 7239, Revision A for toxicity. Bonds well to variety of substrates. One to one mix ratio by weight. Moderate viscosity. Serviceable from -60°F to +250°F. Excellent electrical insulator. Non-halogenated system. |
|
EP93AOFR Two component high strength flame retardant epoxy system that meets stringent horizontal burn test portion of the FAR standard 14 CFR 25.853(a). Non-halogenated system serviceable from -80°F to +300°F. Forgiving one to one mix ratio by weight. Good electrical insulation. |
|
EP93FRHT Two part epoxy system that passes Airbus specifications for flame resistance, smoke density and toxicity. Bonds well to a variety of substrates including metals, composites, glass, ceramic and many plastics. One to one mix ratio by weight. Moderate viscosity. Service operating temperature range from -80°F to +400°F. Excellent electrical insulator. Non-halogenated system. |
|
MasterSil 156 Two part silicone potting/encapsulation compound. Superior thermal conductivity. High elongation. Long pot life. Cures in thicknesses beyond 1-2 inches. UL 94V-0 flame retardant system. Serviceable from -65°F to +221°F. |
|
MasterSil 707FR-NV One component non-corrosive paste produces fast cures at room temperature. Passes UL 94V-1 and 94V-0 testing for flame retardancy. Outstanding adhesion to metals, ceramics, glass and many plastics. Exceptionally soft. |
|
MasterSil 708FR Flowable, no mix, one component RTV silicone compound. Shore A Hardness 30-40. Fast setting at room temperature. Meets requirements of UL 94V-1 and 94V-0 for flame retardancy. Elongation of 200-300%. Gray color. |