Two Component Clear, Long Pot Life Epoxy Adhesive for High Performance General Purpose Bonding
Two Component Clear, Long Pot Life Epoxy Adhesive for High Performance General Purpose Bonding
Master Bond Polymer Adhesive EP21LP is a two component, clear epoxy adhesive for general purpose bonding formulated to feature long pot life at room temperature and cure at room temperature or more rapidly at elevated temperatures, with a one-to-one mix ratio, weight or volume. It readily develops a high bonding strength of more than 3000 psi at room temperature which unlike that of many other epoxy adhesives, is relatively insensitive to mixing ratio or substrate cleaning procedures. Master Bond Polymer Adhesive EP21LF can be applied readily after simple mixing of the two components on many different surfaces. It produces durable high strength and tough bonds which are remarkably resistant to thermal cycling and chemicals including water, oil and most organic solvents, over the exceptionally wide temperature range of -60°F to more than 250°F. Adhesion to metals, glass, ceramics, wood, vulcanized rubbers and many plastics is excellent. The hardened adhesive is an electrical insulator. Color of part A clear amber, part B clear tan. Master Bond EP21LP adhesive is widely used in the electronic, electrical, computer, construction, metalworking, appliance, automotive and chemical industries.
Explore more products...
- Epoxy |
 - Chemically Resistant |
 - Electrically Insulative |
 - Thermal Cycling Resistant |
 - Heat Cure |
 - Room Temperature Cure |
 
			      