Two component, thermally conductive, electrically insulative, cryogenically serviceable epoxy

EP29LPSPAO-1 Black Two Part Epoxy

Key Features

  • Good flow properties
  • Can withstand cryogenic shock
  • High dimensional stability
  • Vacuum compatible