EP41S-F Product Information | MasterBond.com

Versatile, two part epoxy system for bonding, sealing, coating and encapsulating

EP41S-F Two Part Epoxy System

Key Features

  • Very fast curing; quick handling time
  • Excellent electrical insulation properties
  • Impressive physical strength properties
  • Convenient processing, gun dispensable