UV15LV Product Information | MasterBond.com

Low viscosity, one component, UV curable epoxy based system

UV15LV One Part UV Curable Epoxy Based Compound

Key Features

  • Exceptionally low viscosity
  • Superior thermal stability
  • Very little shrinkage upon cure
  • Cationic curing system