630 products match
|
EP29LPAOHT Two component epoxy system featuring good thermal conductivity along with being electrically isolating. It is a low to moderate viscosity system with excellent flow properties. It can be mixed in masses over a gallon because it generates an exceptionally low exotherm. High modulus, outstanding compressive strength, and a low coefficient of thermal expansion. The service temperature range is -60°F to +350°F. |
|
EP29LPHE Low viscosity epoxy for large potting/encapsulation applications. Low modulus, high elongation. Long working life. Exceptionally low shrinkage upon cure. Impressive optical clarity. Low exotherm. Serviceable from -60°F to +250°F. |
|
EP29LPHT Low viscosity, optically clear epoxy for bonding, sealing, potting. Room temperature curing. Superior dielectric properties. Serviceable from -60°F to +300°F. Cures rigid. Long working life. Low shrinkage upon cure. Ideal for large volume potting. |
|
EP29LPSP Two part epoxy system with ultra low viscosity and remarkable cryogenic properties. Withstands rapid drop in temperature and is NASA low outgassing approved. Optically clear. Long working life. Low exotherm. Excellent resistance to acids, bases and many solvents. Outstanding electrical insulative properties. Service operating temperature range from 4K to +275°F. |
|
EP29LPSPAO Low exotherm potting/encapsulation compound. Heat curing two component thermal conductive/electrical insulative system. Can withstand cryogenic shocks. Superior electrical insulation properties. Good chemical resistance. High dimensional stability. Vacuum compatible. Service operating temperature range from 4K to +275°F. |
|
EP29LPSPAO-1 BLACK Thermally conductive/electrically insulative epoxy for bonding, sealing, potting. Good flow properties. Serviceable from 4K to +250°F. Can withstand cryogenic shocks. High dimensional stability. Complies with NASA low outgassing specifications. Black color. |
|
EP29LPSPND-3 Two part epoxy system with paste consistency and remarkable cryogenic properties. Withstands rapid drop in temperature. Long working life. Low exotherm. Excellent resistance to acids, bases and many solvents. Outstanding electrical insulative properties. Service operating temperature range from 4K to +250°F. |
|
EP29LPTCHT Two component epoxy featuring a low viscosity with excellent flow properties. It is electrically insulative and thermally conductive with an impressive fine particle size filler material. Bond line thicknesses range from 5 to 15 microns. |
|
EP3 One component heat curable epoxy adhesive. Fast cure speeds. Resists vibration, impact, stress fatigue cracking, creep corrosion. Gray color. Adhesive spreads evenly and smoothly. Serviceable from -100°F to +300°F. |
|
EP30 Low viscosity two part high performance epoxy resin system. High strength rigid bonds. Low linear shrinkage after cure. Superb optical clarity and light transmission properties. Serviceable from -60°F to +250°F. Cures readily at room temperature. Withstands 1,000 hours 85°C/85% RH. |