442 products match
|
UV15DC80Med USP Class VI approved one component UV and heat curable epoxy. Passes ISO 10993-5 cytotoxicity testing. Cures at temperatures as low as 80°C. Moderate viscosity. Minimal shrinkage upon cure. Capable of withstanding liquid sterilants, radiation, autoclaving. Serviceable from -60°F to +400°F. |
|
UV15DC80ND UV and heat curable epoxy formulation. Cures in "shadowed out" areas at temperatures as low as 80°C. Passes 1,000 hours at 85°C/85% humidity. Convenient no mix system. Serviceable from -60°F to +350°F. Superb electrical insulator. |
|
UV15DC80TK UV and heat curable epoxy formulation. Cures in "shadowed out" areas at temperatures as low as 80°C. Passes 1,000 hours at 85°C/85% humidity. Convenient no mix system. Serviceable from -60°F to +350°F. Superb electrical insulator. |
|
UV15FL Low viscosity epoxy system with enhanced toughness. Substantial temperature resistance, especially when post cured with heat. 100% reactive. Shore D hardnes >75. Tensile strength >5,000 psi. Optically clear, spin coatable. Serviceable from -80°F to +350°F. |
|
UV15LV Low viscosity, high strength epoxy resin based formulation. Enhanced thermal stability. Cationic curing system. Excellent light transmission properties. Superb electrical insulation characteristics. Serviceable from -80°F to +300°F. |
|
UV15RCL Red colored UV curable epoxy system turns clear upon exposure to UV light. Low viscosity, with superb thermal stability. Also capable of spin coating. Outstanding optical clarity. High bond strength. Serviceable from -80°F to +350°F. |
|
UV15TK Moderate viscosity single part UV curable epoxy. Cures quickly. Excellent dimensional stability. Enhanced temperature resistance. Cationic curing system. Optically clear. Volume resistivit >1014. Serviceable from -80°F to +400°F. |
|
UV15X-2 For bonding, sealing, coating, encapsulation. Fast curing no mix compound. Excellent abrasion resistant. Viscosity 3,000-9,000 cps. Shore D hardnes >70. Impressive physical strength properties. Serviceable from -80°F to 300°F. |
|
UV15X-2GT One part, UV curable epoxy with ultra fast curing. Good physical properties and chemical resistance. Used for glob top applications. Thixotropic paste viscosity. Excellent toughness. Withstands thermal cycling. Shore D hardness 65. Serviceable from -80°F to +250°F. |
|
UV15X-5 Tough, abrasion resistant UV curing urethane acrylate type system. Non-yellowing capabilities. Resists thermal cycling and mechanical shocks. Elongatio >200%. Very fast curing. High viscosity. Serviceable from -80°F to +250°F. |