EP39-2LV Product Description

EP39-2LV Two Component Epoxy

Low Viscosity, Fast Curing, Two High Performance Optical Epoxy For Bonding, Sealing, Coating & Casting Featuring Excellent Chemical Resistance

EP3FL Product Information

EP3FL One Part Epoxy Compound

One Component, Thermal Shock and Heat Resistant, Flexibilized Epoxy System for Bonding, as well as for Potting and Encapsulations up to ¼ Inch Thick; Features Good Toughness and Fast Cures.

EP3HT Product Information

EP3HT One Part Epoxy

One Component, Epoxy System for Bonding, Sealing and Coating Featuring Very Fast Cure along with High Shear Strength Properties.

EP3HTS Product Information

EP3HTS One Part Epoxy

One Component, Heat Curing, Silver Filled, Electrically Conductive Epoxy Adhesive/Sealant Featuring High Shear Strength and Good Temperature Resistance Along With a Rapid Cure Speed.

EP3HTSMed Product Information

EP3HTSMed One Part Medical Grade Epoxy

One Component, Heat Curing, Silver Filled, Electrically Conductive Epoxy Adhesive/Sealant Featuring High Shear Strength and Good Temperature Resistance Along With a Rapid Cure Speed

EP3RR-1 Product Description

EP3RR-1 One Part Epoxy

One Part, Lower Viscosity, Thermally Conductive Epoxy System for High Performance Potting, Encapsulation and Underfill Applications Featuring Exceptional Dimensional Stability and Rapid Curing at 230-250°F.

EP3RRLV Product Information

EP3RRLV epoxy adhesive

One Part, Lower Viscosity, Thermally Conductive Epoxy System for High Performance Potting, Encapsulation and Underfill Applications Featuring Exceptional Dimensional Stability and Rapid Curing at 230-250°F.

EP41S Product Information

EP41S Two Part Epoxy System

Two Component Epoxy Resin System for Durable, High Performance,
High Strength Coatings, Liners and Sealants Featuring Chemical Resistance and Fast Cure.

EP41SMed Product Information

EP41SMed Two Component Epoxy System

Two Component Low Viscosity Epoxy System For High Performance Bonding, Sealing, Coating. Including Small Encapsulations, Pottings & Castings Featuring Fast Set-Up and Handling Time Meets USP Class VI and ISO 10993-5 Specifications for Medical Applications.

EP50-1.5 Product Information

EP50-1.5 Two Component Epoxy

Two Component Epoxy Adhesive For Very Fast Cure, High Performance General Purpose Bonding