High Temperature Resistant | Page 3 | MasterBond.com

MasterSil 913Med Product Information

MasterSil 913Med Silicone System

One Component, Room Temperature Curing Silicone Elastomer Adhesive
for High Performance Bonding and Sealing. Fast Curing and Non-Corrosive.

UV15X-6NM-2BCL Product Information

Blue colored UV system for high performance bonding, sealing and coating, turns from blue to clear upon exposure to UV light. Moderate Viscosity, Reliable thermal and electrical insulation. Flexible and tough

UV15 Product Information

UV15 One Part UV Curable Compound

Low Viscosity, One Component, UV Curable Epoxy Based System for High Performance Bonding, Coating and Sealing with Exceptional Thermal Stability and Very Low Shrinkage upon Cure.

UV15RCL Product Information

Red colored UV curable epoxy system

Low Viscosity, One Component, UV Curable Epoxy Based System for High Performance Bonding, Coating and Sealing that turns from red to clear upon exposure to UV light. with Exceptional Thermal Stability and Very Low Shrinkage upon Cure.

MasterSil 323S-LO Product Information

Master Bond MasterSil 323S-LO Silicone System

Two component, silver filled silicone with superb electrical conductivity along with good heat transfer properties.

UV10TK Product Information

One Component, Moderate Viscosity UV Curable System for High Performance Bonding, Sealing and Encapsulating, Featuring Excellent Physical Properties, Dimensional Stability and Chemical Resistance with an Outstanding Tg

EP62-1HTMed Black Product Information

Two Component Epoxy System Features a Very Long Pot Life at Ambient Temperatures Combined with Rapid Cures and Sterilization Resistance, Passes 10993-5 for Cytotoxicity

MasterSil 323Med Product Information

Two Component, medical grade silicone for bonding, sealing and encapsulating. Featuring ISO 10993-5 and excellent strength properties.

MasterSil 323AO-LO Product Information

Two part silicone for high performance casting, potting & encapsulation and sealing

Supreme 11ANHT-2 Product Information

Supreme 11ANHT-2 Two Part Epoxy

Two component, thermally conductive, electrically insulating epoxy for bonding, coating and sealing featuring small particle size filler